This is the outer, which is Arylate and not Aramid. Loki and Yinhe make the same choice, Arylate/ALC for Outer/Viscaria clones, and Aramid/KLC for Inner/Long V clones.
No, Aromatic is used for the same thing than Aramid : KLC. The w81 inner is not Arylate. Loki is pretty clear about that : https://flbook.com.cn/c/VubLi8CH4p
Because quality could be better. I like my AliExpress Lining replicas, but I have to admit that they evacuate sweat less efficiently than my Adidas tennis shirts. I coud want to pay more for a better shirt.
It's not evident because it's not at all. It's a normal Arthur China less tacky. So far from a ESN rubber. Kunlun Sponge II is no tensor at all. And green package exist since at least beginning of 2024.
It's KLC 1nd not ALC. The outer are ALC though.
And only the Loki Arthur King have Super carbon, even the W81 SP has 'normal' carbon : https://flbook.com.cn/c/VubLi8CH4p